MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Novec™ 7000 Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature automated test equipment & wafer processing equipment.

Features and Benefits:

  • Low Global Warming Potential
  • Excellent dielectric properties
  • Non-ozone depleting
  • Low toxicity
  • Non-flammable
  • Non-corrosive
  • Good thermal stability
  • Useful at extreme low temperatures (to -120 Degree C)
  • Will not damage electronic equipment in event of leakage or other equipment failure

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccLiquid
 1.47 g/cc
@Temperature 0.000 °C
 1.70 g/cc
@Temperature -60.0 °C
 1.81 g/cc
@Temperature -120 °C
Kinematic Viscosity 0.32 cSt
 0.28 cSt
@Temperature 30.0 °C
 0.50 cSt
@Temperature -20.0 °C
 1.1 cSt
@Temperature -60.0 °C
 2.0 cSt
@Temperature -80.0 °C
 4.0 cSt
@Temperature -100 °C
 17 cSt
@Temperature -120 °C
Molecular Weight 200 g/mol
Vapor Pressure 0.646 bar
Surface Tension 12.4 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 24.8 bar
Critical Temperature 165 °C
Critical Density 0.553 g/cc
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+8 ohm-cm
Dielectric Constant 7.4
Dielectric Strength 40.0 kV/in
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 142 J/gLatent
CTE, linear 2190 µm/m-°C
Specific Heat Capacity 0.845 J/g-°C
@Temperature -120 °C
 1.04 J/g-°C
@Temperature -60.0 °C
 1.24 J/g-°C
@Temperature 3.00 °C
Thermal Conductivity 0.0750 W/m-K
 0.0720 W/m-K
@Temperature 40.0 °C
 0.0880 W/m-K
@Temperature -40.0 °C
 0.100 W/m-K
@Temperature -100 °C
Boiling Point 34.0 °C
@Pressure 0.101 MPa
 
Descriptive Properties
Solubility35%of air in fluid
 60 ppmwof water in fluid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Novec™ 7100 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 774 Engineered Fluid
Thionyl Chloride, SOCl2
3M Novec™ 71DA Engineered Fluid

PMM33097 / 167844

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.