MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Torque Fluid
Categories: Fluid; Lubricant

Material Notes: Chevron Torque Fluid is a high performance hydraulic fluid designed for use in transmissions and hydraulic systems requiring a fluid meeting the Allison C4 specification

It is manufactured using highly refined base oils, oxidation and corrosion inhibitors, antiwear and extreme pressure agents, and foam suppressant.

Applications

Chevron Torque Fluid is recommended for use in Allison Powershift transmissions, some torque converters, and hydraulic systems requiring an Allison C4 fluid.

It is also recommended for heavy duty truck and tractor automatic transmissions requiring a fluid of its viscosity and general characteristics, and for mobile hydraulic systems where operating requirements are too severe for straight mineral oils.

Key Words: CPS Number: 226705; MSDS Number: 4641
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.3 °
Viscosity 3000 cP
@Temperature -20.0 °C
Cold Crank
Viscosity Measurement 110Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 236 SUS
Saybolt Viscosity at 210°F 50 SUS
Kinematic Viscosity at 40°C (104°F) 45.8 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.0 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -38.0 °CASTM D97
Flash Point 219 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV053 / 74668

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.