MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® 339 Polyester Film, 700 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.

Typical Applications: Melinex® 339 is used as a base for pressure sensitive labels, photographic printing paper, in security and access cards, in multiple use tickets and in general printing applications.

Approvals: UL recognized - Product has been registered with Underwriters Laboratories

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccASTM D1505
Thickness 7.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12000 psiASTM D882A
Film Tensile Strength at Yield, TD 12000 psiASTM D882A
Film Elongation at Break, MD 115 %ASTM D882A
Film Elongation at Break, TD 90 %ASTM D882A
Film Tensile Strength at Break, MD 22000 psiASTM D882A
Film Tensile Strength at Break, TD 23000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 1.5 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
Shrinkage, TD 1.5 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Gloss 40 %45°; ASTM D1003
 45 %60°; ASTM D1003
 
Descriptive Properties
Yield (nominal)2800 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 339 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 357 Polyester Film
DuPont Teijin Films Melinex® 340 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 339 Polyester Film, 820 Gauge

PDTZ9057 / 139452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.