MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Encapsulated Flake Composite
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Carbon Fiber Filled

Material Notes: Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based net-works of CNS with a distinctive morphology that, when added to polymers, elastomers and thermoplastics, enhance the resulting products with multifunctional properties, such as increased conductivity and dramatically improved strength and modulus. These properties allow for the replacement of metal parts with CNS-infused thermoplastics containing a very small amount of CNS, which result in significant cost savings.

Property data is for PC/ABS w/ added 3% CNS by weight

Information provided by Applied Nanostructured Solutions (ANS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.135 g/cc
Thickness 10.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 87.0 MPa
Tensile Modulus 4610 MPa
Flexural Strength 125 MPa
Flexural Modulus 3510 MPa
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 40 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
3% CNS; ASTM D4935
 50 dB
@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
3% CNS; ASTM D4935
 51 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
5% CNS; ASTM D4935
 60 dB
@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
5% CNS; ASTM D4935
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 2.0 %
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) >= 93 %
 
Descriptive Properties
% Sizing, type~4%Polyurethane, Polyimide, Polyamide
Chop Length70µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Covestro Bayblend® ET3036 FR PC/ABS Blend
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend
Covestro Bayblend® FR3000 PC/ABS Blend
Overview of materials for PC/ABS + Stainless Steel

PANS002 / 176022

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.