Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes. Availability: North America Features: - Balanced Stiffness/Toughness
- Good Heat Aging Resistance
- Good Impact Resistance
- Good Processability
- Medium Molecular Weight
- Nucleated
Uses: - Appliances
- Automotive Applications
- Compounding
Processing Method: Blow Molding, Compound and Injection MoldingInformation provided by ExxonMobil |