MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials PE 500 HMW-PE FG HMW-PE FG White High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Polyethylene PE 500 High Molecular Weight HMW-PE FG (Food Grade) is a versatile grade that offers a unique combination of stiffness, toughness, mechanical damping capabilities, great machinability, and moderate wear and abrasion resistance. In less demanding applications with respect to wear and impact resistance, PE 500 may present an economical alternative to standard UHMW grades. Due to these benefits and characteristics in combination with a EU 10/2011 and FDA 21 CFR § 177.1520 Food Contact compliancy, PE 500 HMW-PE FG components are primarily used in the meat and fish processing industry, but can also be found in a variety of mechanical, chemical, and electrical applications.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183-1
Water Absorption 0.10 %
@Time 86400 sec
Immersion; ISO 62
Water Absorption at Saturation 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ISO 868
Tensile Strength, Ultimate 28.0 MPaISO 527-1/-2
Elongation at Break 50 %ISO 527-1/-2
Elongation at Yield 10 %ISO 527-1/-2
Modulus of Elasticity 1.30 GPaISO 527-1/-2
Flexural Strength 27.0 MPaISO 178
Compressive Yield Strength 12.0 MPa
@Strain 1 %
ISO 604
 18.5 MPa
@Strain 2 %
ISO 604
 26.5 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 300 µm/kmISO 7148-2
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 2.50 J/cm²double 14° notched; ISO 21304-2
 10.5 J/cm²partial break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.30Pin-on-disk vs. steel; 0.33 m/s; ISO 7148-2
Sand Slurry 350based on TIVAR®1000 = 100; ISO 15527
Limiting Pressure Velocity 0.0500 MPa-m/sec1 m/s; cylindrical sleeve bearings
 0.0800 MPa-m/sec0.1 m/s; cylindrical sleeve bearings
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistivity per Square 1.00e+12 ohmANSI/ESD STM 11.11
Dielectric Strength 45.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
Melting Point 135 °CDSC, 10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °CContinuous (20.000 hrs)
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °CISO 75-1/-2
Minimum Service Temperature, Air -100 °C
Flammability, UL94 HB
@Thickness 3.00 mm
Oxygen Index 20 %ISO 4589-1/-2
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM943 / 320680

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.