MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance. PEARLCOAT® 161K is used in melt coatings on textile substrates, for end-uses in industrial coatings (for life-jackets, etc.) obtained by extrusion and calendering.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76ASTM D2240
Tensile Strength, Yield 3632 psiASTM D412
Elongation at Break 650 %ASTM D412
50% Modulus 3.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 0.580 ksi
@Strain 100 %
ASTM D412
300% Modulus 1.015 ksi
@Strain 300 %
ASTM D412
Tear Strength 400 pliASTM D624 (Die C)
Abrasion 25Resistance (mm³); DIN 53.516
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 58.0 °CISO 306 (A50)
 
Processing PropertiesOriginal ValueComments
Zone 1 160 °C
Zone 2 170 °C
Zone 3 180 °C
Zone 4 184 °C
Adapter Temperature 185 °C(5)
Die Temperature 185 °C(6)
 185 °CTIP (7)
Drying Temperature 90.0 °C
Dry Time 3.00 - 4.00 hour
Dew Point -40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer

PMES76 / 88453

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.