MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Good Physical Properties and Reduced Surface Tack.

Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection Molding

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0014 cm/cmInjection
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
ASTM D2240
Tensile Strength 44.8 MPaASTM D412
Elongation at Break 570 %ASTM D412
100% Modulus 0.00620 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0110 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 4200 psiASTM D790
Tear Strength 130 pliTrouser; ASTM D470
Graves Tear Strength 450 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 21H18, 1000g; ASTM D3389 B
Tensile Set 19 %200% elongation; ASTM D412/D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °C
 145 °CKofler
Glass Transition Temp, Tg -46.0 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 193 °CInjection
Middle Barrel Temperature 204 °CInjection
Front Barrel Temperature 216 °CInjection
Nozzle Temperature 216 °CInjection
Zone 1 176 °CExtrusion
Zone 2 183 °CExtrusion
Zone 3 188 °CExtrusion
Zone 4 194 °CExtrusion
Adapter Temperature 194 °CExtrusion
Die Temperature 194 °CZone 1, Extrusion
 194 °CZone 2, Extrusion
Melt Temperature 216 °CInjection
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 3000 - 7000 MPaInjection
Back Pressure 50.0 MPaInjection
Screw Speed 20 - 50 rpmInjection
 
Descriptive Properties
Volume Swell in Water1.7%24h/23°C, ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NEU NEUSoft™ 455-50A Ester/ether TPU / SBC blend
Ravago Petrochemical Ravathane® R210A93UV Ether-Based Thermoplastic Polyurethane
RTP Company RTP 1200 T-70A UV Ether-based Thermoplastic Polyurethane Elastomer (; UV Stabilized
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Covestro Platilon® 4201 AU Polyurethane (Ether) Film

PNOVEON047 / 55314

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.