MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

MITO™ RES-1 AND TRI-HDNR KIT Bis A Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: MITO® RES-1 is a Bis A Epoxy resin formulated for high strength, and modified with MITO E-GOTM, the first-of-its kind functionalized graphene additive. MITO® Res-1 is designed for compression molding applications. The high strength and reactivity properties of this product make it an excellent choice for manufacturing high performance sporting goods such as snowboards, skis and paddles. When used with the recommended TRI-HDNR catalyst, excellent low temperature, flexural, impact, damping, and adhesion properties are achieved.

Information provided by Mito Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Brookfield Viscosity 12000 - 14000 cP12000 - 14000 cP
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.6 - 82.2 °C150 - 180 °FTemperature for Cure
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorBlack
Mix Ratio4 : 1 with Catalyst
Volume Solids100%
Weight Solids100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITO02 / 318005

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.