MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Celstran® PA66-GF20-02P11/12 Nylon 66, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Nylon 66 reinforced by 20 weight percent long glass

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.296 g/cc0.04682 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5mm/min; ISO 527-2/1A
Tensile Strength 103 MPa
@Temperature 80.0 °C
14900 psi
@Temperature 176 °F
ISO 527-1, -2
Elongation at Break 1.6 %1.6 %5mm/min; ISO 527-2/1A
 2.6 %
@Temperature 80.0 °C
2.6 %
@Temperature 176 °F
ISO 527-1, -2
Tensile Modulus 8.30 GPa1200 ksi50mm/min; ISO 527-2/1A
 4.97 GPa
@Temperature 80.0 °C
721 ksi
@Temperature 176 °F
ISO 527-1, -2
Flexural Strength 190 MPa27600 psiISO 178
 175 MPa
@Temperature 80.0 °C
25400 psi
@Temperature 176 °F
ISO 178
Flexural Modulus 7.10 GPa1030 ksiISO 178
 4.40 GPa
@Temperature 80.0 °C
638 ksi
@Temperature 176 °F
ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
@Temperature -30.0 °C
9.99 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact Unnotched 4.10 J/cm²19.5 ft-lb/in²ISO 179/1eU
 5.20 J/cm²
@Temperature -30.0 °C
24.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 2.40 J/cm²11.4 ft-lb/in²ISO 179/1eA
 2.70 J/cm²
@Temperature -30.0 °C
12.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 238 °C460 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 285 - 295 °C545 - 563 °F
Zone 2 290 - 300 °C554 - 572 °F
Zone 3 300 - 310 °C572 - 590 °F
Zone 4 300 - 315 °C572 - 599 °F
Die Temperature 300 - 315 °C572 - 599 °F
Melt Temperature 300 - 315 °C572 - 599 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 120 - 150 MPa17400 - 21800 psi
Hold Pressure 50.0 - 80.0 MPa7250 - 11600 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  25 rpm
@Diameter 75.0 mm
25 rpm
@Diameter 2.95 in
 35 rpm
@Diameter 55.0 mm
35 rpm
@Diameter 2.17 in
 50 rpm
@Diameter 40.0 mm
50 rpm
@Diameter 1.57 in
 
Descriptive Properties
Heat stabilized/stable to heatYes
Injection speedmedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry)
Trinseo Magnum™ 3453 Acrylonitrile Butadiene Styrene (ABS)
BASF Ultraform® H 2320 006 Q600 POM
Envalior Akulon® S223-G4U PA66-GF23, Dry, 23% Glass Filled
Envalior Akulon® S223-G4U PA66-GF23, Conditioned, 23% Glass Filled

PHCQ160 / 178615

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.