MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis KOBLEND HI 10 PBT+PC, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Symbol according to ISO 1043/1: PBT+PC-HI

Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents.

Main application fields: automotive industry, bumpers

Unfilled. Suitable for Injection Molding. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: Polybutylene Terephthalate Polyester + Polycarbonate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 250 °C
2.2 g/10 min
@Load 4.76 lb,
Temperature 482 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi50 mm/min
Elongation at Break >= 50 %>= 50 %Nominal
Elongation at Yield 4.6 %4.6 %50 mm/min
Tensile Modulus 1.40 GPa203 ksi1 mm/min
Izod Impact, Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Izod Impact, Notched (ISO) 40.0 kJ/m²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °F
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C124 °F
Vicat Softening Point 105 °C221 °F50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Samyang Triloy® 120H PC/ABS alloy
INEOS Styrolution Terluran® HI-10 ABS
Kingfa LONOY 1200 PC/PBT Alloy
Kingfa LONOY 2100 LT PC/PET Alloy
Chi Mei Polylac® PA-757 ABS

PENJ00 / 35889

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.