MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water quenching. Alloys CLC 17-13-3LN exhibits austenitic microstructure free of deleterious carbide precipitations in grain boundaries. The grade contains residual ferrite (= 2%) after solution annealing (1050 - 1150°C / 1922 - 2102°F) and water quenching. Higher Molybdenum content improves uniform and localized corrosion resistance. Nitrogen additions improve the structure stability and increase the yield strength compared to CLC 17-12-2L. Main properties of CLC 17-13-3LN are : high ductility, easy weldability, mirror polishability. Typical applications are food and beverage processing industry, chemical industry and chemical tankers.

Information provided by manufacturer.

Key Words: EURONORM 1.4429 X2CrNiMoN17.13.3, AFNOR Z3CND 17.12Az, DIN W 1.4429, ASTM A240 TP 316LN, UNS S31653
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.95 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 637 MPaTypical
 580 - 780 MPaMinimum Guaranteed
Tensile Strength, Yield >= 280 MPa
@Strain 0.2 %
 >= 320 MPa
@Strain 1 %
 355 MPa
@Strain 0.2 %
Typical
Elongation at Break >= 45 %
 58 %Typical
Creep Strength 270 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
Modulus of Elasticity 200 GPa
@Temperature 20.0 - 100 °C
Poissons Ratio 0.299Calculated
Shear Modulus 77.0 GPa
@Temperature 20.0 - 100 °C
Charpy Impact >= 187 J
 325 JTypical
 >= 125 J
@Temperature -196 °C
 250 J
@Temperature -196 °C
Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 16.5 µm/m-°C
@Temperature 20.0 - 200 °C
 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
 18.0 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.030 %
Chromium, Cr 17.9 %
Iron, Fe 68.51 %As remainder
Molybdenum, Mo 2.6 %
Nickel, Ni 10.8 %
Nitrogen, N 0.16 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 316LN Stainless Steel, Composition Spec
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
AISI 316N Cast Stainless Steel, UNS J92804
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Cast Stainless Steel CF3MN, ASTM A351

NINDUST08 / 17546

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.