MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Information provided by FIBERFIL Engineered Plastics, now an A. Schulman product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Melt Flow 19 g/10 min230/2.16 (typical); ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6960 psiISO 527
Elongation at Yield 2.5 %ISO 527
Flexural Strength 10660 psiISO 178
Flexural Modulus 420 ksiISO 178
Izod Impact, Notched (ISO) 4.10 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 19.5 kJ/m²ISO 180/1U
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 103 Z Polypropylene (PP), Glass Fiber - FDA Compliant Ingredients
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
A. Schulman Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
LATI Latene® 3 TG/300 30% Mineral/Glass Fiber Filled Polypropylene Homopolymer (PPH)
LATI Latene® 9H CI/301 30% Glass Sphere Filled, Heat Stabilized Polypropylene Homopolymer (PPH)

PFIBFIL64 / 38249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.