MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 4544 Polyester Carvable Wood Filler
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: This polyester resin base compound is easy to use, sets in minutes and can be sanded or carved almost immediately. Acts like wood yet exhibits no grain problems. BC4544 Wood Filler can be carved, sanded, filed, scraped, drilled, tapped or machined to a featheredge. No paint preparation is required and even accepts stain better than wood.
APPLICATIONS: Tooling: A must for the wood tooling, model and pattern industry, making revisions, engineering changes and rebuilding of wood pattern and master models. Marine: Ideal for patching holes in hulls and bulkheads. An excellent water resistance item for emergency repairs for all types of wood and fiberglass boats. Furniture: For the restoration of all types of wood furniture and antiques. Seals and fills in holes, gouges and cracks. Great for the furniture refinisher. Other Applications: A unique lightweight filler paste designed for working with model craft and other wood products in any scale or form.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 - 60.0 min
@Temperature 24.0 °C
0.333 - 1.00 hour
@Temperature 75.2 °F
Pot Life 6.0 - 12 min
@Temperature 24.0 °C
6.0 - 12 min
@Temperature 75.2 °F
1lb mass
Shelf Life 12.0 Month12.0 Monthin tightly closed container
 
Descriptive Properties
Mix Ratio100:1 or 100:2 resin/hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Industeel FORA 360 BC 360 HB Wear Resistant Steel
Goodfellow Hot Pressed Boron Carbide B4C
Boron Carbide, B4C
BCC Products BC 4553 Polyester Styling Paste

PBCC001 / 107228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.