MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger DELRIN® 511 Series Acetal Homopolymer POM-H
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes:
  • good machinability
  • high stiffness
  • high fatigue strength
  • high creep resistance
  • good wear properties
  • very good abrasion resistance
Target Industries:
  • automotive industry
  • food engineering
  • construction industry
  • conveyor technology
  • mechanical engineering
  • electronics
  • fixture construction
  • home appliances
  • gear manufacturing

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³
Moisture Absorption 0.900 %0.900 %saturation; ASTM D570
 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D 785
Tensile Strength, Yield 68.9 MPa10000 psiASTM D 638
Elongation at Break 25 %25 %ASTM D 638
Elongation at Yield 18 %18 %ASTM D 638
Modulus of Elasticity 3.10 GPa450 ksiASTM D 638
Flexural Strength 110 MPa16000 psiASTM D 790
Flexural Modulus 3.59 GPa520 ksiASTM D 790
Compressive Yield Strength 114 MPa
@Strain 10 %
16500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 14.5 MPa
@Strain 1 %
2100 psi
@Strain 1 %
ASTM D 695
Izod Impact, Unnotched 0.667 J/cm1.25 ft-lb/inASTM D 256
Coefficient of Friction, Dynamic 0.35
@Pressure 0.276 MPa
0.35
@Pressure 40.0 psi
50 fpm; ASTM D 3702
Coefficient of Friction, Static 0.20
@Pressure 0.276 MPa
0.20
@Pressure 40.0 psi
ASTM D 3702
K (wear) Factor 11.1 x 10-8 mm³/N-M5.50 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D 3702
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 122 µm/m-°C68.0 µin/in-°FASTM D 696
Specific Heat Capacity 1.46 J/g-°C0.350 BTU/lb-°F
Melting Point 178 °C352 °FDIN EN ISO 11357
Maximum Service Temperature, Air 85.0 °C185 °FLong Term
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FISO-R 75 Method A
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8132 / 319060

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.