MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK 843-1 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Silver

Product Benefits:

  • One component
  • Solvent-free
  • Electrically conductive
  • High purity
  • Strong bond strength
  • Screen printable
  • Syringe dispensable
Cure: Heat cure

Application: Die attach

LOCTITE ABLESTIK 843-1 electrically conductive die attach adhesive has been formulated for use in high throughput, automated die attach equipment. This adhesive is ideal for application by syringe dispensing or screen printing. LOCTITE ABLESTIK 843-1 adhesive provides strong bonds and is designed to withstand thermal compression wire bonding.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 8500 cPUncured
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 10.3 MPa
@Temperature 350 °C
Die, 50 mil²
 27.6 MPa
@Temperature 25.0 °C
Die, 50 mil²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00020 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µm/m-°CCured, Below Tg
 120 µm/m-°CCured, Above Tg
Thermal Conductivity 2.07 W/m-K
@Temperature 121 °C
Cured
Glass Transition Temp, Tg 76.0 °CCured
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 170 °C
 30.0 min
@Temperature 150 °C
Alternate Cure Schedule
Shelf Life 3.00 Month
@Temperature 25.0 °C
Uncured, from date of manufacture
 6.00 Month
@Temperature 5.00 °C
Uncured, from date of manufacture
 12.0 Month
@Temperature -40.0 °C
Uncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)10Cured, Sodium (Na+)
 5Cured, Potassium (K+)
 5Cured, Chloride (Cl-)
Weight Loss (%)0.22Cured @ 250ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5010 / 255221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.