MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 2200 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Glass Fiber- and Kevlar-Reinforced, Epoxy-Novolac; High Strength, Excellent Abrasion and Corrosion Resistance

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/cc
Viscosity 165000 cPMixed
Linear Mold Shrinkage 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Flexural Strength 13400 psiASTM D790
Shear Strength 2300 psiASTM D1002-94
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 4.7
@Frequency 1000 Hz
Dielectric Strength 460 V/mil
Dissipation Factor 0.010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µin/in-°F
@Temperature 20.0 °C
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -67.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 175 °C
Alternate Cure
 24.0 - 48.0 hour
@Temperature 23.0 °C
Recommended Cure
Pot Life 42.0 min
@Temperature 25.0 °C
100 gm mass
 
Descriptive Properties
Chemical ResistanceGood
ColorRust Brown
Mix Ratio by Weight1:1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlisle 201HD Carbon-Carbon Composite
General Plastics LAST-A-FOAM® TR-15 Polyurethane Foam
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets

PAREM11 / 24275

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.