MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Pellethane® 2363-80AE TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pellethane 2363-80AE is a thermoplastic polyurethane elastomer

Features: USP Class VI

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0040 cm/cmASTM D955
Melt Flow 10 g/10 min
@Load 8.70 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ASTM D2240
Tensile Strength, Ultimate 4200 psiASTM D412
Elongation at Break 650 %70% Elongation set after break; ASTM D412
50% Modulus 4.80 MPa
@Strain 50 %
ASTM D412
100% Modulus 6.10 MPa
@Strain 100 %
ASTM D412
300% Modulus 10.3 MPa
@Strain 300 %
ASTM D412
Tear Strength 73.6 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
@Load 1.00 kg
H-22 (coarser); ASTM D1044
Compression Set 30 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395
 80 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
CTE, linear 165 µm/m-°CASTM D696
Vicat Softening Point 81.7 °CASTM D1525
Glass Transition Temp, Tg -47.0 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 188 - 204 °CExtrusion
 188 - 204 °CMolding
Mold Temperature 16.0 - 60.0 °C
Drying Temperature 82.0 - 93.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 2363-80A TPU
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
Lubrizol LifeSciences Pellethane® 2363-90AE TPU
Lubrizol LifeSciences Carbothane® PC-3595A-B20 Aliphatic TPU

PLUBR9029 / 203596

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.