MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Preliminary Data Sheet

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
Filler Content 30 %Unspecified
Water Absorption 0.90 %
@Thickness 0.318 mm
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.8 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 110 MPaASTM D790
Flexural Modulus 3720 MPaASTM D790
Izod Impact, Notched 35.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 265 °CASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 60.0 - 107 °C
Drying Temperature 82.2 °C
Dry Time 4.00 hour
 
Descriptive Properties
Filler / ReinforcementGlass Bead
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityNorth America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Nymax™ GB 1200 20 HS BLACK 18 Polyamide 66 (Nylon 66)
Avient Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6), DAM
Avient Edgetek® ET6620-0020 FRV0 Polyamide 66 (Nylon 66)

PH0POL0668 / 145237

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.