MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt SMC 4500 R23 Sheet Molding Compound
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: SMC 4500 R23 is a sheet molding compound based on an unsaturated polyester resin reinforced with glass fibers. This SMC has been developed for sink and tray application. SMC 4500 R23 joints good mechanical properties with stain and chemical resistance. SMC 4500 R23 has been studied to show a decorative effect on the part molded. SMC 4500 R23 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Filler Content 23 %23 %Glass; ISO 11667
Water Absorption <= 0.20 %<= 0.20 %ISO 62 Met. 1
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ISO 2039-2
Flexural Strength 130 MPa18900 psiISO 14125A
Flexural Modulus 9.50 GPa1380 ksiISO 14125A
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FISO 75
 
Processing PropertiesMetricEnglishComments
Mold Temperature 140 - 160 °C284 - 320 °F
Hold Pressure 6.998 - 11.00 MPa1015 - 1595 psiMolding pressure
 
Descriptive Properties
Molding time40 s/mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9115 / 231710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.