MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
APCM DA 4090/4092 Epoxy Pregpreg System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DA 4090 and DA 4092 are modified epoxy pre-impregnated systems which can cure at 250°F (121°C) for one hour. DA 4090 and DA 4092 can be supplied on any commercially available glass, Kevlar, or graphite fabric. DA 4090 is a one sided pre-impregnated fabric yielding a single sided tack material. DA 4092 is the same system where both sides of the fabric are pre-impregnated yielding a double sided tack material. Both prepreg systems can be used for laminating and honeycomb sandwich construction.

Mechanical Properties: Based upon 0.125 inch thick cured laminate consisting of DA 4090 on 7781 glass cloth cured at 250°F (121°C) for one hour.

Information provided by Adhesive Prepegs for Composite Manufacturers, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 63400 psiASTM D638
Tensile Modulus 3.50e+6 psiASTM D638
Flexural Strength 80100 psiASTM D790
Flexural Modulus 3.00e+6 psiASTM D790
Compressive Strength 48600 psiASTM D695
Shear Strength 7450 psiInterlaminar; ASTM D2344
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 121 °C
Shelf Life 1.00 Month
@Temperature 22.2 °C
 6.00 Month
@Temperature 4.44 °C
 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
SeparatorRelease paper and poly film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
APCM DA 4080/4082 Epoxy Pregpreg System
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Hexcel® HexTow® AS7 12K Standard Modulus Carbon Fiber
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Hexcel® HexTow® AS4 3K Standard Modulus Carbon Fiber (3000 Filaments)

PAPCM002 / 187015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.