MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexForce™ 352 Aramid Fabric  (discontinued **)
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramids display excellent dimensional stability with a slightly negative coefficient of thermal expansion (-2.4 X 10-6/ºC.) They are resistant to chemicals with the exception of a few strong acids and alkalis.
Aramids have excellent stability over a wide range of temperatures for prolonged periods. They show essentially no embrittlement or strength loss at temperatures as low as -320ºF (-196ºC). Aramids do not melt or support combustion but will start to carbonize at approximately 800ºF (427ºC).

Information provided by Hexcel

Key Words: Kevlar
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 9.30 mil
Fiber Count 1140 denierWarp yarn; Kevlar® 49
 1140 denierFill yarn; Kevlar® 49
 
Mechanical PropertiesOriginal ValueComments
Tensile Impact 624 ft-lb/inWarp
 643 ft-lb/inFilling
 
Thermal PropertiesOriginal ValueComments
CTE, linear -2.40 µm/m-°C
Maximum Service Temperature, Air 427 °Cstarts to carbonize
Minimum Service Temperature, Air -196 °C
 
Descriptive Properties
Fabric Weight (oz/yd2)5.1Dry
Nominal Construction (count/in)17Warp
 17Fill
Weave StylePlain

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel® F161 Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin

PHEXC489 / 101108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.