MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is generally characterized by improved processability in polymer forming technologies where stretching flows occur.

Materials, such as paper and board, coated with Daploy WF420HMS have high grease resistance. They can be submerged in boiling water for a certain period of time without deterioration. Daploy WF420HMS can be used in microwave oven applications. With a considerably low coating weigh a practically pinholes-free coating can be achieved.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 230 °C
DIN 5335/ISO 1133
Neck In 7.00 cmBTM 00115
Coating Weight 10.0 g/m²BTM 00117
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1.55 GPaISO 527
Charpy Impact, Notched 0.350 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 162 - 165 °CISO 3146
Vicat Softening Point 153 °CA/50 (10 N); ISO 306
 
Optical PropertiesOriginal ValueComments
Gloss 100 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion
Borealis Daploy™ WB140HMS Polypropylene
Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion
Borealis Daploy™ WB180HMS Polypropylene

PBOREA172 / 27479

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.