MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL LL6F 802-HSB Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL® LL6F 802-HSB is an ethylene 1-hexene LLDPE resin with good stiffness at thin gauges, good drawdown and excellent processability. This resin is suitable for blown and cast film applications and for blends with LLDPE or HDPE.

Recommended Applications: Stretch wrap, overwrap, coextrusions, blown film and cast film.

Additives: Antiblock – 6250 ppm, Slip – 1000 ppm, processing aid.

Form(s): Pellets.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 6250 ppm
Slip Level 1000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1250 psiASTM D882
Film Tensile Strength at Yield, TD 1450 psiASTM D882
Film Elongation at Break, MD 580 %ASTM D882
Film Elongation at Break, TD 780 %ASTM D882
Flexural Modulus, 1% Secant 200 MPaMD; ASTM D882
 214 MPaTD; ASTM D882
Coefficient of Friction 1.0ASTM D1894
Elmendorf Tear Strength MD 300 gASTM D1922
Elmendorf Tear Strength TD 550 gASTM D1922
Dart Drop Test 140 gASTM D1709A
Film Tensile Strength at Break, MD 6200 psiASTM D882
Film Tensile Strength at Break, TD 4800 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 °CASTM D3418
Vicat Softening Point 95.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D1003
Gloss 140 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO134 / 283731

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.