MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Picco™ A-10 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Picco™ A-10 Hydrocarbon Resin is a low molecular weight, resinous plasticizer derived largely from aromatic petroleum feedstock. Picco™ A-10 Hydrocarbon Resin is characterized by its chemical inertness, excellent resistance to salts, acids, alkalies, water and brines and its solubility in a wide variety of hydrocarbon solvents. Picco™ A-10 Hydrocarbon Resin is indicated for use as a binder in lithographic (cold set) inks and as plasticizer, softener and tackifier for other resins and elastomers used in rubber compounding and various adhesive systems.

Application/Uses:

  • Caulks and Sealants
  • Contact Adhesives
  • Graphic Arts
  • Hot Melt Adhesives
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Waterborne Adhesives
  • Wire and Cable
Key Attributes:
  • Excellent pigment wetting
  • Excellent resistance to acids, alkalis and moisture
  • Liquid plasticizer and tackifier
  • Non-reactive
  • Soluble in a wide variety of hydrocarbon solvents

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 5500 cP
@Temperature 40.0 °C
LVTD, spindle 31
Molecular Weight 420 g/molMn
 750 g/molMw. Mw/Mn ratio = 1.8
 1850 g/molMz
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 9.0ASTM D6166
 
Descriptive Properties
Cloud Point0°COMS
 106°CDACP
 -24°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5527 / 222721

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.