Applications include cold drawn or finished bar, cold punched nuts, split rivets, machine screws, and wood screws. Post oil quenched hardness: 48 HRC surface, 43 HRC half-radius, 38 HRC center. |
UNS G11410, ASTM A29, ASTM A107, ASTM A108, ASTM A311, FED QQ-S-637, SAE J403, SAE J412, SAE J414 |