MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPE ME-2570B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2500 series are super high flow, high density, high performance thermoplastic elastomer designed for demanding exterior automotive applications, including window encapsulation. Sarlink ME-2570B is a medium hardness, high density injection molding grade excellent UV resistance and adhesion to glass with primer.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion Good Flexibility; Good Processability; Good Surface Finish; Good Toughness; High Density; High Flow; High Specific Gravity; Medium Hardness; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Viscosity 123 cP
@Shear Rate 206 1/s,
Temperature 200 °C
123 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  70
@Time 5.00 sec
70
@Time 0.00139 hour
ISO 868
 74
@Time 1.00 sec
74
@Time 0.000278 hour
ISO 868
Tensile Strength at Break 5.90 MPa856 psiFlow; ISO 37
 6.50 MPa943 psiAcross Flow, 20 mm/mm; ISO 37
 5.79 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
839 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 7.28 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1060 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  2.10 MPa
@Strain 100 %
305 psi
@Strain 100 %
Across Flow, 20 mm/mm; ISO 37
 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 730 %730 %Flow; ISO 37
 800 %800 %Across Flow, 20 mm/mm; ISO 37
 815 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
815 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 896 %
@Treatment Temp. 125 °C,
Time 605000 sec
896 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tear Strength 28.0 kN/m160 pliFlow; ISO 34-1
 28.0 kN/m160 pliAcross Flow, Method Ba, Angle (Unnicked; ISO 34-1
Compression Set  22 %
@Temperature 22.8 °C,
Time 79200 sec
22 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 76 %
@Temperature 90.0 °C,
Time 252000 sec
76 %
@Temperature 194 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °F
Middle Barrel Temperature 175 - 195 °C347 - 383 °F
Front Barrel Temperature 180 - 205 °C356 - 401 °F
Nozzle Temperature 180 - 205 °C356 - 401 °F
Melt Temperature 180 - 205 °C356 - 401 °F
Mold Temperature 15.0 - 40.0 °C59.0 - 104 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1081 / 237572

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.