MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Trilliant™ HC X THC 1101 Natural Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Trilliant™ HC blends made with Tritan™ copolyester are available in standard grades or can be customized to meet specific performance requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0056 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0045 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.4 MPaType I, 51 mm/min; ASTM D638
Tensile Strength, Yield 41.4 MPa51 mm/min; ASTM D638
Elongation at Break 40 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 1740 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 74.5 MPa13 mm/min; ASTM D790
Flexural Modulus 1900 MPa13 mm/min; ASTM D790
Izod Impact, Notched 850 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Descriptive Properties
FeaturesGood Chemical Resistance
 Good Color Stability
 Good Flow
 Good Toughness
 High Impact Resistance
 Hydrolytically Stable
 Medium Heat Resistance
FormsPellets
Generic MaterialCopolyester
Generic NameCopolyester
Regional AvailabilityAfrica & Middle East
 Europe
 North America
 South America
UsesElectrical Housing
 Hospital Goods
 Housings
 Medical Appliances
 Medical/Healthcare Applications
 Thin-walled Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ MX731 Medical Grade Copolyester
Avient Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)
Avient Trilliant™ HC X THC 1100 Natural Copolyester
Avient Versaflex™ OM 2262 Thermoplastic Elastomer (TPE)
Eastman Tritan™ LX100 Copolyester

PH0POL1096 / 145665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.