MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake EF600 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Westlake EF600 is a fractional melt LDPE with excellent toughness. This material contains zero slip and zero anti-block. It is recommended in heavy duty films and shipping sacks and in industrial shrink applications. It can be used as a bubble stabilizer in LLDPE rich films. Applications: Heavy duty bags, Heavy duty shipping sacks, Industrial shrink film, Heavy duty C&A sheeting.

Test specimens for blown film: nominal thickness 2.5 mils; blow up ratio 2.5:1, die gap 35 mils at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D1505
Melt Index of Compound 0.18 g/10 min0.18 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 830 %830 %ASTM D882
Coefficient of Friction 1.51.5ASTM D1894
Dart Drop 10.2 g/micron260 g/milASTM D1709
Film Tensile Strength at Break, MD 30.3 MPa4400 psiASTM D882
Film Tensile Strength at Break, TD 27.6 MPa4000 psiASTM D882
1% Secant Modulus, MD 241 MPa35000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 238 °C410 - 460 °FWith blow-up ratios of 1.5:1 or higher.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8725 / 287835

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.