MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, friable to tough, and contains no free chemicals. All oxides and dioxides are combined chemically as follows: Fe2O3Al2(SiO4)3. The iron and aluminum are partially replaceable by calcium, magnesium and manganese. There are three types- aluminum garnet, iron garnet & chromium garnet.
Uses: Abrasive applications, water jet cutting, water filtration, tumbling media, non-skid surfaces, and semi-precious stone.
Forms Available: Sintered pieces, targets, granules and various powder sizings

Information provided by Reade Advanced Materials.

Key Words: Fe3Al2(SiO4)3, Iron aluminum silicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.90 - 4.10 g/cc3.90 - 4.10 g/cc
Bulk Density 2.40 g/cc0.0867 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 8.0 - 9.08.0 - 9.020°C
 
Thermal PropertiesMetricEnglishComments
Melting Point 1250 - 1315 °C2280 - 2399 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.74 - 1.891.74 - 1.89
 
Descriptive Properties
Colorred to pink
Crystal Structurecubic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Lutetium Aluminum Garnet:Cerium (LAG:Ce) Scintillator Crystal
Calcium Fluoride, CaF2 (Fluorite)
Harris Acoustic Sensors ELL-1203 Aluminum Substituted Narrow Line Width Garnet (3-Series)
Mateck Calcium Fluoride (CaF2)
SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)

CREADE011 / 1945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.