MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon™ 858G-917 Permeation Resistant PFA Coating
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon™ perfluoroalkoxy (PFA) industrial coatings melt and flow during baking to provide nonporous films. These multi-coat systems provide higher continuous use temperatures (260 °C [500 °F]), have a high dielectric strength, and are considered tougher than PTFE or FEP. Because of their chemical resistance properties, Teflon™ PFA industrial coatings can be used on pumps, tanks, valves, and vessels used in the chemical processing industry. These coatings also provide nonstick properties suitable for industrial bake ware applications. Teflon™ PFA industrial coatings come in a robust line of water-based liquid and powder forms.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Thickness 3.00 - 6.00 milFilm Build per coat
 <= 40.0 milMax Total Film Build
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 391 °CCure Temperature
 
Compliance PropertiesOriginal ValueComments
FDA NoFood Contact per 21CFR.
 
Descriptive Properties
CarrierWater
Chemical/Solvent ResistanceExcellentASTM D543
ColorRuby Red
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8722 / 268648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.