MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Forplast PEHD P 131 (PC) PE 80 Post-Consumer Recycled HDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: PE grade code: High Density Polyethylene recycled (Post-Consumer Recycled)

Stabilization recipe: Antacid, antioxidant thermostabilized processing aid, dispersing agent carbon black.

Application: Pipe coating and cable protection

Information provided by Forplast Srl.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 - 0.960 g/cc0.0341 - 0.0347 lb/in³Compound; ISO 1183
ESCR 100% Igepal® >= 300 hour>= 300 hourD1693
ESCR 10% Igepal® >= 1000 hour>= 1000 hourD1693
Oxidative Induction Time (OIT)  >= 10 min
@Temperature 220 °C
>= 10 min
@Temperature 428 °F
ISO 11357
 >= 30 min
@Temperature 210 °C
>= 30 min
@Temperature 410 °F
ISO 11357
Carbon Black Loading >= 2.0 %>= 2.0 %ASTM D1603
Melt Flow 0.30 - 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 - 1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
UNI 1133T
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60UNI EN ISO 868
Tensile Strength, Yield >= 15.0 MPa>= 2180 psi50mm/min; UNI 5819
Elongation at Break >= 600 %>= 600 %50mm/min; UNI 5819
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FASTM D 2117
Vicat Softening Point 118 °C
@Load 1.02 kg
244 °F
@Load 2.25 lb
A/50; ASTM D 1525
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D 746
 
Descriptive Properties
Supply formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFORP903 / 316414

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.