MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Astralloy Rol-Man® Wear Resistant Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Rol-Man® is a high manganese, fully austenitic, quench annealed, non-magnetic, work hardening steel with an exceptionally high level of wear resistance when subjected to work-hardening by shock or high impact pressure while in service. The main characteristic of Rol-Man is superior wear resistance. Severe wear on the surface has a work-hardening effect on the austenitic structure of this steel. This leads to an increase in hardness from 200 BHN (in as delivered plates) up to an in-service hardness of at least 600 BHN. This work-hardening capability renews itself throughout its in-service life. The underlayers which are not work-hardened maintain an excellent resistance to shock and a very high ductility.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 220220As Furnished
 600600Work Hardened for Service
Tensile Strength 938 MPa136000 psi
Tensile Strength, Yield 379 MPa55000 psi
Elongation at Break 40 %
@Thickness 50.8 mm
40 %
@Thickness 2.00 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.0 - 1.4 %1.0 - 1.4 %
Iron, Fe 84.2 - 87.9 %84.2 - 87.9 %As Balance
Manganese, Mn 11 - 14 %11 - 14 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si 0.10 - 0.30 %0.10 - 0.30 %
Sulfur, S 0.010 - 0.030 %0.010 - 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wingate Alloys Winco Mang 11-14% Manganese, Work Hardening Steel
AISI Type S24000 Stainless Steel, plate
205 Austenitic Stainless Steel (UNS S20500)

NNUCOR905 / 233179

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.