MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese FORTRON 1132L4 PPS, Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes:

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psi50mm/min; ISO 527-2/1A
Elongation at Break 2.0 %2.0 %50mm/min
Flexural Strength 260 MPa37700 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Izod Impact, Notched (ISO) 9.30 kJ/m²4.43 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1131L4 ITT PPS, 30% Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese FORTRON 317 PPS, Unfilled
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Celanese FORTRON 1130L0 PPS, 30% Glass Reinforced

PHCQ268A / 183216

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.