Key Properties: - Excellent adhesive for low surface energy plastics without primer.
- Used in potting, painting and protective coating applications.
- Excellent thermal and mechanical shock resistance.
- Ease of use.
Applications: Flexible to 130% elongation, good chemical resistance. Bonds to most plastics, rubber, polyurethane, metals, ceramic and concrete. Tough, flexible, chemically resistant, non-blush clear coating with medium gloss finish. Potting compound alternative to castable polyurethanes, particularly for electrical cable/connector/transducer termination. Excellent for electrical and electronic applications as protective encapsulate against very wide range of environmental exposures, particularly moisture and sea water. Can be applied to oily surfaces. Will cure underwater. Ambient cure 24 hours or 3 hours at 100°C for full cure. |