Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Injection Molding Forms: Pellets Additive: Impact Modifier Information Provided by Teknor Apex |