MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Betamate™ 5103-2 Epoxy Adhesive, Body Shop Grade
Categories: Polymer; Thermoset; Epoxy

Material Notes: BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated steels, is resistant to degradation and to substrate corrosion on environmental aging. The product is precurabel to induction and compatible with electro-coat paint process.

This former Dow product line is now a DuPont product line. Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Solids Content >= 98 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 6000 MPaISO 527-1/-2
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 180 °C
Shelf Life 3.00 Month
@Temperature <=30.0 °C
 
Descriptive Properties
BasisEpoxy resin
Colorlight green
CompatibilityMetals
Extrusion Viscosity73 to 7325°C, Ford nozzle d=3 mm / 3 bar
PolymerAdhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow BETAMATE™ 1045 Epoxy
DuPont Mobility and Materials Betamate™ 1496V Epoxy Adhesive, Body Shop Grade
Dow BETAMATE™ 7000/7050 L Epoxy
DuPont BETAMATE™ 73345G Epoxy
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide

PDTF9092 / 30214

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.