MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics VELECRETE RC 103 Rodding Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in compliance with international standards.

Bond: Ultrafine

Aggregate: Sintered Mullite

Type of Setting: Hydraulic

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.50 g/cc0.0903 lb/in³After Drying at 110°C
Porosity 16 - 18 %
@Temperature 1300 °C
16 - 18 %
@Temperature 2370 °F
Grain Size <= 10000 µm<= 10000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0130 GPa
@Temperature 1000 °C
1.89 ksi
@Temperature 1830 °F
Cold
 0.0150 GPa
@Temperature 1100 °C
2.18 ksi
@Temperature 2010 °F
Hot
 0.0180 GPa
@Temperature 1400 °C
2.61 ksi
@Temperature 2550 °F
Cold
 0.0180 GPa
@Temperature 110 °C
2.61 ksi
@Temperature 230 °F
Cold
Compressive Strength  65.0 MPa
@Temperature 1000 °C
9430 psi
@Temperature 1830 °F
Cold Crushing
 90.0 MPa
@Temperature 110 °C
13100 psi
@Temperature 230 °F
Cold Crushing
 90.0 MPa
@Temperature 1400 °C
13100 psi
@Temperature 2550 °F
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.63 W/m-K
@Temperature 600 °C
11.3 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Hot Face
Maximum Service Temperature, Air 1600 °C2910 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 60 %60 %
Fe2O3 1.2 %1.2 %
 
Descriptive Properties
Permanent Linear Change<-0.7%1600°C
Thermal Expansion0.9at 1100°C
Thermal Shock ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSHARA045 / 130208

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.