MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addolink® 1701 Crosslinking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Information: Liquid aromatic diamine crosslinker for polyurethane/polyurea and epoxy systems. It shows a higher reactivity than Addolink 1708 and glycolic crosslinkers.

Function: Addolink 1701 is a low viscous aromatic diamine for chain extending high quality polyurethane and polyurea systems. Main applications are RIM, spray coatings and cold cast systems.

Application:

  • RIM two component PU systems (Reaction Injection Molding)
  • PU and Polyurea spray coatings
  • PU One Shot systems
  • PU sealant systems
  • PU Rigid Foam
  • Epoxy resins

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Viscosity 330 cP330 cPDIN 53015
Molecular Weight 178 g/mol178 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 20.0 - 25.0 °C
6.00 Month
@Temperature 68.0 - 77.0 °F
 
Descriptive Properties
Appearanceyellow-brown to dark brown liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8204 / 208597

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.