MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; PC/ABS + Stainless Steel; Polycarbonate (PC)

Material Notes: EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0070 cm/cm0.0055 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psi
Elongation at Break 2.2 %2.2 %
Tensile Modulus 5.50 GPa798 ksi
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm100 ohm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °F
Vicat Softening Point 125 °C
@Load 5.00 kg
257 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Electromagnetic reflection92 dB
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MRC Polymers NAXALOY™ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced
LATI LASTILAC 11 ABS/PC-Based Alloy
LATI Lastilac 10 ABS/PC
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy

PLATH9963 / 177659

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.