SP001 is high purity polymeric semiconductor P3HT. SP001 is suitable for applications such as organic photovoltaics and organic electronics devices and can be used in either top gate or bottom gate device configuration. Application areas include Bulk transport devices, Organic photovoltaics (OPV), Organic electronic (OE) devices, Field effect transistors (FET) |