MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ V 3050D-S0097 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolefin phase with a cross-linked EPDM phase dispersed within it. This range of compounds are specially formulated to provide the melt strength and processability required for blow-moulding processes. In addition to this, OnFlex™-V 3000 series thermoplastic elastomer compounds provide excellent colourability (low yellowness), good mechanical properties, excellent flexibility over a wide temperature range, a wide hardness range, and good hydrocarbon, heat ageing and weather resistance.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ISO 868
Tensile Strength at Break 16.2 MPa2350 psiISO 37
Tensile Stress at Strain  8.50 MPa
@Strain 100 %
1230 psi
@Strain 100 %
ISO 37
 10.0 MPa
@Strain 300 %
1450 psi
@Strain 300 %
ISO 37
Elongation at Break 600 %600 %ISO 37
Compression Set  45 %
@Temperature 23.0 °C,
Time 259000 sec
45 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 70 %
@Temperature 70.0 °C,
Time 79200 sec
70 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 75 %
@Temperature 100 °C,
Time 79200 sec
75 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
FeaturesGeneral Purpose
FormsPellets
Generic MaterialTPE
Generic Material TypeThermoplastic Vulcanizate (TPV)
Generic NameThermoplastic Elastomer (TPE)
Injection RateFast
Processing MethodBlow Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE)
Avient OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Avient OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE)

PH0POL0768 / 145337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.