MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gamma Titanium Aluminide, TiAl
Categories: Metal; Intermetallic

Material Notes: Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability. A range of stoichiometries is possible through elemental substitutions. Researchers are examining titanium aluminide applications in fields such as jet engine turbines because of their high temperature properties and low density.

May be processed by ingot metallurgy or forging. Limited processability by casting. Difficult to sheet roll.


Composition table gives weight percent.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.91 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 450 - 800 MPa
Tensile Strength, Yield 400 - 650 MPa
Elongation at Break 0.00 - 4.0 %
Modulus of Elasticity 176 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 1460 °C
Maximum Service Temperature, Air 900 °COxidation Limit
Maximum Service Temperature, Inert 1000 °CCreep Limit
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 36 %
Titanium, Ti 64 %
 
Descriptive Properties
Critical Ordering Temperature1460°C
Crystal StructureL10Ordered Tetragonal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Aluminide, TiAl3
Alpha-2 Titanium Aluminide, Ti3Al
Special Metals INCONEL® Alloy 718
Titanium, Ti
Ti-24Al-11Nb Titanium Aluminide

MIAL010 / 12199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.