MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LyondellBasell Purell PE 3420F Low Density Polyethylene (LDPE)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Purell PE 3420F is the latest generation of low density polyethylene with extremely high rigidity and outstanding temperature resistance. It is delivered in pellet form. The grade is used for packaging of pharmaceuticals in the small blow molding market e.g. produced with Blow Fill Seal technology. Applications: Blow-Fill-Seal Applications, Bottles and Vials, Caps & Closures (Healthcare), Healthcare Applications, Medical Devices, Medical Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 31.2 lb/ft³ISO 60
Density 0.933 g/ccISO 1183-1
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 15.0 MPaISO 527-1,-2
Elongation at Yield 11 %ISO 527-1,-2
Tensile Modulus 520 MPaISO 527-1,-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 119 °CDSC; ISO 3146
Vicat Softening Point 111 °CA50N; ISO 306
 
Descriptive Properties
Processing MethodBlow, Fill, & Seal, Blown Film, Extrusion Blow Molding, Injection Blow Molding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2910M Low Density Polyethylene
LyondellBasell Hostalen GX 5058 High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Purell PE 3040D Low Density Polyethylene (LDPE)
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade

PEQT8636 / 220270

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.