MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast; Nylon 6, Impact Grade

Material Notes: TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of nylon with the impact-resistance of the modifier. TECAST VEKTON™ 6PB cushion pads are brilliant OSHA orange to provide easy identification.

  • Excellent shock load characteristics protect expensive hammer anvils
  • High energy transmittance effectively uses hammer force to drive pile

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110 - 115
Tensile Strength, Yield 9300 - 10600 psi
@Temperature 22.8 °C
Modulus of Elasticity 370 - 425 ksi
@Temperature 22.8 °C
Compressive Strength 11500 - 13000 psi
@Temperature 22.8 °C
at 1% Deformation
Shear Strength 6500 - 7500 psi
@Temperature 22.8 °C
Izod Impact, Notched 0.800 - 1.00 ft-lb/in
@Temperature 22.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECAST™ Cast Nylon (PA)
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6)
High-Leaded Tin Bronze, UNS C93500, Copper Casting Alloy
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6)
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6)

PENSIN030 / 92847

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.