MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar and steel. Adhesive strength is maintained even in cryogenic conditions. This resilient adhesive can also be used for tacking wires and as a protective coating. TRA-BOND 724-14C adhesive exhibits good dielectric properties. There are several cure options, including curing at room temperature. It contains a fluorescent trace for inspection purposes.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccMixed
Viscosity 500000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
Adhesive Bond Strength 1700 psiLap shear, alum to alum
Peel Strength 20.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cm
Dielectric Constant 7.0
@Frequency 1000 Hz
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 0.250 g/min15 gauge needle @ 80 psi
Cure Time 1.00 hour
@Temperature 93.0 °C
 3.00 hour
@Temperature 74.0 °C
 72.0 hour
@Temperature 25.0 °C
Working Life 30.0 min
@Temperature 25.0 °C
Shelf Life 3.00 Month
@Temperature -40.0 °C
 
Descriptive Properties
Color Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 724-20 Polyurethane Adhesive
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive

PTRAC143 / 71071

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.