MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or more rapidly at elevated temperatures. The outstanding feature of EP76M-F focuses on the faster set up time and full cure of the system when compared to the more standard EP76M. However, it should be noted that EP76M-F has a more limited open time. Unlike the majority of two part nickel conductive systems, EP76M-F has a one to one mix ratio by weight or volume and has no solvents or diluents. It has a paste consistency and is easy to apply. The volume resistivity of the cured system is 5-10 ohm-cm. EP76M-F is particularly noteworthy for its strength profile along with good resistance to chemicals including water, oil, and many acids and bases. EP76M-F has a wide temperature range of -60°F to +2 50°F. Adhesion to metals, composites, ceramics, glass, vulcanized rubbers and many plastics is excellent. Parts A and B are both colored gray. Master Bond EP76M-F is widely used in the electronic, electrical, computer and related industries where shielding and static dissipation are prime requirements, along with faster curing times.

Product Advantages:

  • Convenient mixing: one to one by weight or volume; contains no volatiles.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly.
  • Versatile cure schedules; ambient temperature cures or fast elevated temperature cures as required.
  • Good electrical and thermal conductivity.
  • High bond strength to similar and dissimilar substrates.
  • Bonds well to a wide variety of substrates, especially metals and composites.
  • Faster set up and cure times.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity >= 500000 cPPart A, thixotropic
 >= 900000 cPPart B, thixotropic
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 80
Tensile Strength at Break >= 6000 psi
Shear Strength >= 1500 psiTensile lap, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.0 - 10 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 45.0 µm/m-°C
Thermal Conductivity 8.00 - 9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 93.3 °C
 24.0 - 48.0 hour
@Temperature 23.9 °C
Pot Life 15 - 20 min100 gram batch
Shelf Life 3.00 - 6.00 Monthunopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTB413 / 149660

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.