MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 650UC Epoxy Ultra Clear
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: The Chem-Set™ 650UC Epoxy Ultra Clear is a medium viscosity, liquid epoxy system for bonding natural stone. It is excellent for seams, lamination, repairs and applications that require a UV-stable, optically-clear appearance that is suitable for interior and exterior use. This epoxy is quick setting and fast curing, with ample working and positioning times. The working time is about four minutes, along with a cure time of an hour. When the appearance of the repair/application is crucial, and a liquid epoxy is required, the Chem-Set™ 650UC is the best opt.

BONDS / ADHERES TO: Stone, metal, glass, ceramics, concrete, and wood in all combinations.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 lb/gal
Viscosity 10000 - 15000 cPmixed
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 1.0 %
Adhesive Bond Strength 2450 psiASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -20.0 °F
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 1.0
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hourFunctional Cure
 24.0 hourFull
Working Life 4.00 min
@Temperature 21.1 °C
 
Descriptive Properties
Appearanceclear
Fixture Time15 minutes
Mix Ratio1 (resin): 1 (hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI921 / 232232

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.