MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox 25-C40 Polymer NAR tert-Butyl peroxypivalate
Categories: Other Engineering Material

Material Notes: Initiator (40% active ingredient in odorless mineral spirits) for (co)polymerization of ethylene. Polyethylene (LDPE). Used for both tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range.

CAS number: 927-07-1

EINECS/ELINCS No: 213-147-2

Applications: Trigonox 25-C40 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.800 g/cc
@Temperature 20.0 °C
0.0289 lb/in³
@Temperature 68.0 °F
 0.900 g/cc
@Temperature 10.0 °C
0.0325 lb/in³
@Temperature 50.0 °F
Half-life  0.100
@Temperature 94.0 °C
0.100
@Temperature 201 °F
[hr]
 1.00
@Temperature 75.0 °C
1.00
@Temperature 167 °F
[hr]
 10.0
@Temperature 57.0 °C
10.0
@Temperature 135 °F
[hr]
Storage Temperature -20.0 - -5.00 °C-4.00 - 23.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 25.0 °C77.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay39.0-41.0 %
Content=0.06%Hydroperoxides as TBHP
 =60 mg/kgInorganic + organic hydrolysable chloride
 3.58-3.77 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1076 / 286599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.