MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayflex® 110-35 IMR Urethane Elastomer, 15% Wollastonite Filled
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex 110-35 IMR system produces a solid urethane elastomer which has a flexural modulus of approximately 33,500 psi* at room temperature.

Properties / Applications: Bayflex 110-35 IMR system produces a solid urethane elastomer which has a flexural modulus of approximately 33,500 psi* at room temperature. This system is used to provide multiple releases of large reaction injection molding (RIM) parts, such as automotive fascias. The system contains internal mold release (IMR) and is used with milled glass fiber or mineral reinforcements. Bayflex 110-35 IMR is a formulated RIM system supplied as two liquid components. Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. As with any product, use of the Bayflex 110-35 IMR system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccPolyol (Component B)
 1.14 g/ccASTM D792
 1.21 g/ccIsocyanate (Component A)
Viscosity 125 cPPolyol (Component B)
 700 cPIsocyanate (Component A)
Linear Mold Shrinkage 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3200 psiASTM D638/ASTM D412
Elongation at Break 75 %ASTM D638/ASTM D412
Flexural Modulus 689 MPa
@Temperature 65.0 °C
ASTM D412
 1030 MPa
@Temperature 23.0 °C
ASTM D412
 1900 MPa
@Temperature -30.0 °C
ASTM D412
Izod Impact, Notched 3.00 ft-lb/inASTM D624
Tear Strength 600 pliDie C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µin/in-°FASTM D696
Flash Point 160 °CPolyol (Component B)
 213 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 66.0 °C
 
Descriptive Properties
AppearanceLight yellow to yellow liquidIsocyanate (Component A)
 Pale yellow liquidPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled
Covestro Bayflex® 110-50 Urethane Elastomer, 25% Glass Filled
Covestro Bayflex® 110-35 IMR Urethane Elastomer, 15% Glass Filled
Covestro Baydur® STR/C 1000 Liquid Structural RIM, 30% Glass Filled

PCOVEST0120 / 201903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.